Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 2.17 kV/mm | >= 55.0 kV/in | At 50 mils; ASTM D149 |
Borealis Superclean™ LE4244 Natural Crosslinkable Polyethylene for HIV Power Cable Insulation Superclean LE4244 is a natural crosslinkable polyethylene compound developed especially for the insulation of medium and high voltage cables. It provides an excellent balance of anon-staining antio.. |
|||
Dielectric Strength | 2.17 kV/mm | 55.0 kV/in | ASTM D149 |
Zircar Refractory Composites RS-101 Refractory Sheet ZRCI Refractory Sheet Type RS-101 is a ceramic fiber reinforced structural alumina product with useful properties to 2300°F (1260°C). It retains strength and utility to levels far exceeding maximu.. |
|||
Dielectric Strength | 2.17 - 49.6 kV/mm | 55.0 - 1260 kV/in | Average value: 31.3 kV/mm Grade Count:58 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |
|||
Dielectric Strength | 2.17 kV/mm | 55.0 kV/in | |
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |