Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.30 kV/mm | 185 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 7.30 kV/mm | 185 kV/in | Step by Step; ASTM D149 |
Plenco 4527 Phenolic, Granular, Injection Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |