Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.10 kV/mm | 180 kV/in | Short Time; ASTM D149 |
Plenco 7200 Phenolic, Granular, Injection Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Dielectric Strength | 7.10 kV/mm | 180 kV/in | |
Du-Co Ceramics DC-65 Cordierite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |