Material Notes:
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
Water Absorption 1.0 - 5.0 %
1.0 - 5.0 %
Porous
Mechanical Properties Metric English Comments
Hardness, Mohs 7.5
7.5
Tensile Strength, Ultimate 48.0 MPa
6960 psi
Flexural Strength 97.0 MPa
14100 psi
Compressive Strength 483 MPa
70100 psi
Impact Test 0.510 J
0.376 ft-lb
unspecified impact test
Thermal Properties Metric English Comments
CTE, linear 2.90 µm/m-°C

@Temperature 20.0 - 650 °C
1.61 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 3.40 W/m-K
23.6 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1100 °C
2010 °F
Safe Operating Temp
Electrical Properties Metric English Comments
Dielectric Constant 6.0

@Frequency 1e+6 Hz
6.0

@Frequency 1e+6 Hz
Dielectric Strength 7.10 kV/mm
180 kV/in
Dissipation Factor 0.0080

@Frequency 1e+6 Hz
0.0080

@Frequency 1e+6 Hz
Dielectric Loss Index 0.048
0.048
1 MHz