Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.4 - 51.2 kV/mm | 365 - 1300 kV/in | Average value: 23.2 kV/mm Grade Count:38 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Dielectric Strength | 14.4 kV/mm | 366 kV/in | 60Hz, Step-by-Step, dry; ASTM D149 |
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron.. |
|||
Dielectric Strength | 14.4 - 15.3 kV/mm | 366 - 389 kV/in | ASTM D149-97a |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | ASTM D149 |
Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass This data represents typical values for the production ma.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QI-18/57-325 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QI-5/16-220 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M SJ-2A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M SJ-3A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D-149 |
3M 5300 Motor Lead Splicing Kits 3M Motor Lead Splicing Kits 5300 Series are a series of kits designed for splicing motor lead cables to incoming feeder cables. The kits accommodate the follow splice confiations:Pigtails (stub) con.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8424-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8425-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8428-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8429-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8429-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8429-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8430-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8452 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8459 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8460 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8462 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QI-10/37-270 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QSLV-M-8-2/0 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M SJ-1A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Dielectric Strength | 14.4 - 16.3 kV/mm | 365 - 415 kV/in | short time |
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres.. |
|||
Dielectric Strength | 14.4 - 16.4 kV/mm | 367 - 417 kV/in | short time |
Bulk Molding Compounds BMC HT12-1027 Unsaturated Polyester Bulk Molding Compound BMC HT12-1027 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8427-16 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8429-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8461 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 14.4 kV/mm | 366 kV/in | 60 Hz, wet, SS; ASTM D149 |
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at.. |
|||
Dielectric Strength | 14.4 - 16.4 kV/mm | 366 - 416 kV/in | short time |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |