Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
127 microns
5.00 mil
Side 1; Arlon SQA-TMS-003
152 microns
6.00 mil
Side 2; Arlon SQA-TMS-003
457 microns
18.0 mil
Substrate; Arlon SQA-TMS-003
737 microns
29.0 mil
Overall; Arlon SQA-TMS-003
Outgassing - Total Mass Loss 0.10 %
0.10 %
Post Cured - CVCM; ASTM E 595
0.28 %
0.28 %
Cured - CVCM; ASTM E 595
0.34 %
0.34 %
Post Cured - TML; ASTM E 595
1.07 %
1.07 %
Cured - TML; ASTM E 595
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
Silicone Property; ASTM D2240
Tensile Strength 5.86 MPa
850 psi
Silicone Property; ASTM D412
Elongation at Break 450 %
450 %
Silicone Property; ASTM D412
Tear Strength 12.3 kN/m
70.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 1.49 kN/m
8.50 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 14.4 kV/mm
365 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 218 °C
2.00 hour

@Temperature 425 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 18.3 - 23.9 °C
6.00 Month

@Temperature 65.0 - 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 28
Arlon SQA-TMS-025