Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.0 - 12.0 kV/mm | 254 - 305 kV/in | |
Permabond UV7141 UV-curable Adhesive Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet.. |