Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.0 - 117 kV/mm | 508 - 2970 kV/in | Average value: 34.1 kV/mm Grade Count:7 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |