Electrical Properties Metric English Comments
Dielectric Strength 10.7 kV/mm
272 kV/in
IEC 60243
Polycasa COPOL PETG
QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v..
Dielectric Strength 10.7 kV/mm
272 kV/in
IEC 60243-1
Polycasa LENTICULAR PETG
Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert..
Dielectric Strength 10.7 kV/mm
272 kV/in
Step by Step; ASTM D149
Plenco 1500 Polyester, Granular, Compression Molded
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon..