Polymer Property : High Amp Arc Ignition, HAI = 69 arcs Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Amp Arc Ignition, HAI 69 arcs

@Thickness 0.800 mm
69 arcs

@Thickness 0.0315 in
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded &
Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high ..