Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15.0 - 30.0 sec | 15.0 - 30.0 sec | Average value: 22.5 sec Grade Count:4 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Hot Wire Ignition, HWI | 7.00 - 30.0 sec | 7.00 - 30.0 sec | Average value: 16.8 sec Grade Count:4 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Hot Wire Ignition, HWI | 7.00 - 30.0 sec | 7.00 - 30.0 sec | Average value: 16.8 sec Grade Count:4 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Hot Wire Ignition, HWI | 7.00 - 30.0 sec | 7.00 - 30.0 sec | Average value: 21.1 sec Grade Count:5 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |