Polymer Property : Hot Wire Ignition, HWI = 15.0 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 15.0 - 30.0 sec
15.0 - 30.0 sec
Average value: 22.5 sec Grade Count:4
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Hot Wire Ignition, HWI 15.0 - 60.0 sec
15.0 - 60.0 sec
Average value: 33.8 sec Grade Count:8
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Hot Wire Ignition, HWI 15.0 - 60.0 sec
15.0 - 60.0 sec
Average value: 41.1 sec Grade Count:25
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Hot Wire Ignition, HWI 15.0 - 120 sec
15.0 - 120 sec
Average value: 72.9 sec Grade Count:22
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Hot Wire Ignition, HWI 15.0 - 120 sec
15.0 - 120 sec
Average value: 75.3 sec Grade Count:26
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..