Polymer Property : Hot Wire Ignition, HWI = 150 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI >= 150 sec
>= 150 sec
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded  
AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d..
Hot Wire Ignition, HWI >= 150 sec
>= 150 sec
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded &
Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high ..
Hot Wire Ignition, HWI >= 150 sec
>= 150 sec
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, Dry As Molded  
AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela..