Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 335 °C | 635 °F | Tc |
CeramTec Sonox® P502 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Curie Temperature | 335 °C | 635 °F | Tc |
CeramTec Sonox® P505 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |