Material Notes:
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications. Sonox® P505 is designed specifically for actuators.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Electrical Properties Metric English Comments
Curie Temperature 335 °C
635 °F
Tc
Dielectric Constant 780
780
e33 S/e?
900
900
e11 S/e?
1850
1850
e11 T/e?
1880
1880
e33 T/e?
Dissipation Factor 0.015
0.015
tand
Piezoelectric Longitudinal Coupling Factor, k33 0.73
0.73
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -180
-180
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 670
670
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 28.5
28.5
Piezoelectric Planar Coupling Factor, kp 0.65
0.65
Piezoelectric Mechanical Q 80
80
Piezoelectric Shear Coupling Factor, k15 0.71
0.71
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 475
475
Piezoelectric Transverse Coupling Factor, k31 0.33
0.33
Descriptive Properties Value Comments
Aging Rates (%/decade) 0.5
Cf
0.6
Ck
-1.6
Ce
Elastic Compliance (10^-12 m²/N) 17.9
s11^E
24
s33^E
Elastic Rigidity (10^10 N/m²) 14.7
c33^D
4
c55^D
Frequency Constants (kHz·mm) 1300
N3
1360
N1
1880
Nt
2010
Np
Piezoelectric Coupling Coefficient, kt 0.53