Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | <= -196 °C | <= -321 °F | |
Special Metals INCOLOY® Alloy 825 A nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as.. |
|||
Curie Temperature | <= -196 °C | <= -321 °F | |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Curie Temperature | <= -196 °C | <= -321 °F | |
Special Metals INCONEL® Alloy 601 A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper.. |
|||
Curie Temperature | <= -196 °C | <= -321 °F | |
Special Metals INCONEL® Alloy 625 Niobium content includes tantalum. A nickel-chromium-molybdenum alloy with an addition of niobium that acts with the molybdenum to stiffen the alloy's matrix and thereby provide high strength witho.. |
|||
Curie Temperature | <= -196 °C | <= -321 °F | |
Special Metals MONEL® Alloy 401 A copper-nickel alloy designed for specialized electrical and electronic applications. It has a very low temperature coefficient of resistance and medium-range electrical resistivity. Used for wir.. |