Magnetic Remanence, Br 5800 - 7200 Gauss
5800 - 7200 Gauss
Ceradyne SEMICORE® S1-5C Specials SmCo5 Samarium Cobalt Magnet
Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal..