Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 5800 - 7200 Gauss | 5800 - 7200 Gauss | |
Ceradyne SEMICORE® S1-5C Specials SmCo5 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |
|||
Magnetic Remanence, Br | 5800 Gauss | 5800 Gauss | |
Alliance BIN-55 Bonded (Composite) Magnetic Material |
|||
Magnetic Remanence, Br | 5800 Gauss | 5800 Gauss | |
Alliance BIS-59 Bonded (Composite) Magnetic Material |