Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 5500 Oe | 5500 Oe | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Magnetic Coercive Force, Hc | 5500 Oe | 5500 Oe | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |