Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 14 Oe
14 Oe
International Mold Steel NAK55 Precipitation Hardened Mold Steel
Description: NAK55 is a precipitation, or age-hardened mold steel with a through hardness of approximately 40 HRc. NAK55 is ideal for use in plastic and rubber molds and other applications where imp..
Magnetic Coercive Force, Hc 14 Oe
14 Oe
International Mold Steel NAK80 Precipitation Hardened Mold Steel
Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, u..