Material Notes:
Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, uniform hardness, and excellent dimensional stability.Unique Characteristics: Super clean, Vacuum-Arc Remelt manufacturing process.40 HRc hardness.Age-hardened for uniformity of hardness throughout, even in heavy sections.When welded, NAK leaves no witness lines after re-aging.Uniform grain structure with no pin holes, inclusions or hard spots.Machines up to 20% faster than 30 HRc P20 mold steels.Never needs stress relieving, even after heavy machining.Polishes to a superior No. 1 finish, even over welded areas.Applications: Clear lens moldsExtremely critical diamond finish applicationsMolds requiring special EDM finishInformation provided by International Mold Steel.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 40
40
Tensile Strength, Ultimate 1264 MPa
183400 psi
Tensile Strength, Yield 1018 MPa

@Strain 0.200 %
147600 psi

@Strain 0.200 %
Elongation at Break 16.1 %
16.1 %
Elongation in 2" (longitudinal)
Reduction of Area 41.9 %
41.9 %
Modulus of Elasticity 207 GPa

@Temperature 23.0 °C
30000 ksi

@Temperature 73.4 °F
Charpy Impact 11.0 J
8.10 ft-lb
V-Notch, Longitudinal
11.5 J
8.50 ft-lb
V-Notch, Transverse
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 20.0 - 100 °C
6.30 µin/in-°F

@Temperature 68.0 - 212 °F
12.6 µm/m-°C

@Temperature 20.0 - 200 °C
7.00 µin/in-°F

@Temperature 68.0 - 392 °F
13.5 µm/m-°C

@Temperature 20.0 - 300 °C
7.50 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 41.33 W/m-K

@Temperature 93.3 °C
286.8 BTU-in/hr-ft²-°F

@Temperature 200 °F
42.19 W/m-K

@Temperature 204 °C
292.8 BTU-in/hr-ft²-°F

@Temperature 400 °F
Component Elements Properties Metric English Comments
Aluminum, Al 1.0 %
1.0 %
Carbon, C 0.15 %
0.15 %
Copper, Cu 1.0 %
1.0 %
Iron, Fe 93.05 %
93.05 %
Manganese, Mn 1.5 %
1.5 %
Nickel, Ni 3.0 %
3.0 %
Silicon, Si 0.30 %
0.30 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 380
<= 380
Magnetic Coercive Force, Hc 14 Oe
14 Oe
Magnetic Saturation Flux Density, Bmax 16360 Gauss
16360 Gauss
Saturate Magnetism
Magnetic Remanence, Br 8500 Gauss
8500 Gauss
Residual Magnetism
Users viewing this material also viewed the following: