Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 1.1 Oe | 1.1 Oe | |
Pacific Sintered Materials FS-1602 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Magnetic Coercive Force, Hc | 1.1 Oe | 1.1 Oe | |
Pacific Sintered Materials FS-1603 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Magnetic Coercive Force, Hc | 1.1 Oe | 1.1 Oe | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1602 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Magnetic Coercive Force, Hc | 1.1 Oe | 1.1 Oe | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1603 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |