Material Notes:
Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.00 - 7.30 g/cc
0.253 - 0.264 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 448 MPa
65000 psi
Elongation at Break 9.5 %
9.5 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 9.1
<= 9.1
K-Gauss/Oe
Magnetic Coercive Force, Hc 1.1 Oe
1.1 Oe
Magnetic Saturation Flux Density, Bmax 11900 Gauss
11900 Gauss
Magnetic Induction
Magnetic Remanence, Br 5100 Gauss
5100 Gauss
Copyright © lookpolymers.com All Rights Reserved