Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 7500 V | 7500 V | Dielectric Strength |
Dielectric Polymers NT-590DL Protective Film
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized Class 392°FHigh temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications:.. |
|||
Dielectric Breakdown | 7500 V | 7500 V | Dielectric Strength |
Dielectric Polymers NT-590 Polyimide Film Tape
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gol.. |
|||
Dielectric Breakdown | 7500 V | 7500 V | |
Saint-Gobain CHR® 2045-2 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | 7500 V | 7500 V | |
Saint-Gobain CHR® K100 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Breakdown | 7500 V | 7500 V | |
3M 93020LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |