Dielectric Polymers NT-590 Polyimide Film Tape  (discontinued **)

Category Polymer , Adhesive , Film , Tape , Thermoset , Polyimide, TS , Silicone
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dielectric Polymers NT-590 Polyimide Film Tape  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gold finger contacts during wave soldering, flame resistant electrical and thermal insulation, wire and cable wrap and wire bundle termination.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Backing
38.1 microns
1.50 mil
Adhesive
Mechanical Properties Metric English Comments
Elongation at Break 60 %
60 %
Peel Strength 0.2849 kN/m
1.625 pli
Adhesion
5.26 kN/m
30.0 pli
Tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
>= 288 °C
>= 550 °F
Shear Adhesive Failure (polyester failure)
316 °C
600 °F
Intermittent
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Dielectric Breakdown 7500 V
7500 V
Dielectric Strength
Descriptive Properties Value Comments
Color Amber