Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 6900 V | 6900 V | |
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |