Dielectric Breakdown 58000 V
58000 V
IPC TM-650 2.5.6
Arlon CLTE-AT Commercial Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing ..
Dielectric Breakdown 58000 V
58000 V
IPC TM-650 2.5.6
Arlon CLTE-XT High Precision Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing ..