Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 22800 V | 22800 V | ASTM D149 |
Plenco 1508 Polyester, Briquette, Injection Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |