Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 21800 V | 21800 V | 1hr 120C; ASTM D149 |
Plenco 08122 Polyester BMC, Compression Molded PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |