Polymer Property : Dielectric Breakdown = 21800 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown 21800 V
21800 V
1hr 120C; ASTM D149
Plenco 08122 Polyester BMC, Compression Molded
PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..