Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 14200 V | 14200 V | 1hr 120C; ASTM D149 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |