Electrical Properties Metric English Comments
Insulation Resistance 8.80e+14 ohm
8.80e+14 ohm
ASTM D257
Unitika UNILATE® 1 PC PET
Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe..