Material Notes:
Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and others, and extruding the composite resins into plates, and laminating and heat-pressing the plates. UNILATE plates and boards are superior in heat resistance, withstand voltage, strength, and processability to the plates and boards of thermoplastic resins such as nylon, polyacetal, and others. The UNILATE plates and boards are greatly improved in water-absorbing property, electrical properties, and processability, compared to other thermosetting resin laminated sheets used in electric insulation applications.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 65.0 MPa
9430 psi
Horizontal; ASTM D570
110 MPa
16000 psi
Vertical; ASTM D570
Elongation at Break 1.9 %
1.9 %
Horizontal; ASTM D570
2.4 %
2.4 %
Vertical; ASTM D570
Flexural Strength 125 MPa
18100 psi
Horizontal; ASTM D790
220 MPa
31900 psi
Vertical; ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
Horizontal; ASTM D790
11.0 GPa
1600 ksi
Vertical; ASTM D790
Compressive Strength 135 MPa
19600 psi
ASTM D695
Shear Strength 64.0 MPa
9280 psi
ASTM D732
Izod Impact, Unnotched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 25.0 - 100 °C
22.2 µin/in-°F

@Temperature 77.0 - 212 °F
Vertical; ASTM D696
74.0 µm/m-°C

@Temperature 25.0 - 100 °C
41.1 µin/in-°F

@Temperature 77.0 - 212 °F
Horizontal; ASTM D696
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Flammability, UL94 HB

@Thickness 0.600 mm
HB

@Thickness 0.0236 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Insulation Resistance 8.80e+14 ohm
8.80e+14 ohm
ASTM D257
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 37.0 kV/mm
940 kV/in
Under ambient atmosphere; ASTM D149
37.0 kV/mm
940 kV/in
After water absorption; ASTM D149
Dissipation Factor 0.025

@Frequency 1.00e+6 Hz
0.025

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
Comparative Tracking Index 275 V
275 V
IEC 112
Descriptive Properties Value Comments
Appearance Opaque
Ignition Temperature 471°C