Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 3.66e+10 ohm | 3.66e+10 ohm | Bellcore, Control - final |
Indium Corp. 3577-TF Wave Solder Flux, No-Clean Wave Solder Flux 3577-TF is a low-solids flux specially formulated to eliminate post-cleaning operations. This flux contains a small amount of resin, which enhances the wetting properties.3577-TF i.. |