Polymer Property : Insulation Resistance = 10.0 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 10.0 - 1.00e+11 ohm
10.0 - 1.00e+11 ohm
Average value: 4.63e+9 ohm Grade Count:24
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Insulation Resistance 10.0 - 1.00e+8 ohm
10.0 - 1.00e+8 ohm
Average value: 2.63e+6 ohm Grade Count:22
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Insulation Resistance 10.0 - 1.00e+14 ohm
10.0 - 1.00e+14 ohm
Average value: 4.13e+12 ohm Grade Count:25
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Insulation Resistance 10.0 - 1.00e+10 ohm
10.0 - 1.00e+10 ohm
Average value: 7.22e+8 ohm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..