Electrical Properties Metric English Comments
Dielectric Strength 3.20 kV/mm

@Thickness >=3.00 mm
81.3 kV/in

@Thickness >=0.118 in
96hr/105°C/+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
Dielectric Strength 3.20 kV/mm

@Thickness >=3.00 mm
81.3 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac..