Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 17.7 kV/mm

@Thickness 1.57 mm
450 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP320 Cotton Fabric
Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape..
Dielectric Strength 17.7 kV/mm

@Thickness 1.57 mm
450 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP509 Glass Fabric
Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc..
Dielectric Strength 17.7 kV/mm

@Thickness 3.20 mm
450 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 457 PBT
6.5% GR PBT, UL94 V-0/5V.
Dielectric Strength 17.7 kV/mm

@Thickness 3.20 mm
450 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific)
6.5% GR PBT, UL94 V-0/5V.
Dielectric Strength 17.7 kV/mm

@Thickness 1.02 mm
450 kV/in

@Thickness 0.0400 in
ASTM-D149
CoorsTek ADS-995 99.5% Alumina Thin Film
Applications: thin film substrates
Dielectric Strength 17.7 kV/mm

@Thickness 1.02 mm
450 kV/in

@Thickness 0.0400 in
ASTM-D149
CoorsTek ADS-996 99.6% Alumina Thin Film
Applications: thin film substrates
Dielectric Strength 17.7 kV/mm

@Thickness 1.02 mm
450 kV/in

@Thickness 0.0400 in
ASTM-D149
CoorsTek Superstrate® 996 99.6% Alumina Thin Film
Applications: thin film substrates
Dielectric Strength 17.7 kV/mm

@Thickness 3.00 mm
450 kV/in

@Thickness 0.118 in
short time, 1/4" electrodes, 500 V/sec; ASTM D149-97a
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM
Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st..