Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
356 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
Short Time; ASTM D149 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
|
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 1.60 mm |
356 kV/in @Thickness 0.0630 in |
|
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
|
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 1.60 mm |
356 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
Dielectric Strength | 14.0 kV/mm @Frequency 60 Hz |
356 kV/in @Frequency 60 Hz |
Wet, short time; ASTM D149 |
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole RX 640 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.Information supp.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm |
356 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |
|||
Dielectric Strength | 14.0 kV/mm @Frequency 60.0 Hz |
356 kV/in @Frequency 60.0 Hz |
step-by-step, dry; ASTM D149 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 2.00 mm |
356 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 2.4%); ASTM-D149 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 2.00 mm |
356 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 2.9%); ASTM-D149 |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 2.00 mm |
356 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 2.4%); ASTM-D149 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.00 mm |
356 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap .. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm, Temperature 95.0 °C |
356 kV/in @Thickness 0.126 in, Temperature 203 °F |
500 V/s, in oil; Short Time; ASTM D149 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |