Electrical Properties Metric English Comments
Shielding Effectiveness 50.0 - 97.0 dB
50.0 - 97.0 dB
Average value: 76.0 dB Grade Count:4
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..