Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 50.0 dB | 50.0 dB | Average value: 50.0 dB Grade Count:3 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Shielding Effectiveness | 50.0 dB | 50.0 dB | Average value: 50.0 dB Grade Count:3 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Shielding Effectiveness | 50.0 - 97.0 dB | 50.0 - 97.0 dB | Average value: 76.0 dB Grade Count:4 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |