Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 65 dB @Frequency 1.00e+7 - 3.00e+9 Hz |
65 dB @Frequency 1.00e+7 - 3.00e+9 Hz |
|
P & P Technology M W Conductive Fabric Material: Nylon/PET/Nickel/Copper. Self Adhesive Tape: Standard double sided acrylic carrier and adhesiveInformation provided by P & P Technology |
|||
Shielding Effectiveness | <= 65 dB | <= 65 dB | Modified IEEE-299 |
Parker Chomerics CHOFORM® 5550 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Shielding Effectiveness | >= 65 dB | >= 65 dB | 10 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer Conductive Elastomer. CHO-SEAL 1260 elastomer is a silver-filled-silicone intended for mounting silicon wafers during processes such as ion milling. It provides high levels of electrical and thermal.. |
|||
Shielding Effectiveness | >= 65 dB | >= 65 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer Conductive Elastomer. CHO-SEAL 1260 elastomer is a silver-filled-silicone intended for mounting silicon wafers during processes such as ion milling. It provides high levels of electrical and thermal.. |
|||
Shielding Effectiveness | >= 65 dB | >= 65 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer Conductive Elastomer. CHO-SEAL 1260 elastomer is a silver-filled-silicone intended for mounting silicon wafers during processes such as ion milling. It provides high levels of electrical and thermal.. |
|||
Shielding Effectiveness | >= 65 dB @Frequency 1.00e+7 - 1.00e+10 Hz |
>= 65 dB @Frequency 1.00e+7 - 1.00e+10 Hz |
|
Parker Chomerics Tecknit Teckfip™ FIP-C Formed in Place Conductive Elastomer Description: This compound is an all round high performance compound, and is very similar to a Consil C molded or extruded elastomer. It has been traditionally used for telecommunications base stati.. |
|||
Shielding Effectiveness | 65 - 68 dB | 65 - 68 dB | ASTM D4935 |
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information .. |
|||
Shielding Effectiveness | 65 - 70 dB @Frequency 2.00e+8 - 1.20e+10 Hz |
65 - 70 dB @Frequency 2.00e+8 - 1.20e+10 Hz |
|
Parker Chomerics CHO-FORM 5541 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Shielding Effectiveness | 65 dB @Frequency 1.00e+7 - 3.00e+9 Hz |
65 dB @Frequency 1.00e+7 - 3.00e+9 Hz |
|
P & P Technology MW Series Conductive Fabric Material: Nylon/PET/Nickel/Copper fabric Self Adhesive Tape: Conductive double sided acrylic carrier and adhesiveInformation provided by P & P Technology |