P & P Technology MW Series Conductive Fabric

Category Metal , Nonferrous Metal , Copper Alloy , Nickel Alloy , Polymer , Thermoplastic , Nylon , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer P & P Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology MW Series Conductive Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material: Nylon/PET/Nickel/Copper fabric Self Adhesive Tape: Conductive double sided acrylic carrier and adhesiveInformation provided by P & P Technology
Mechanical Properties Metric English Comments
Abrasion 5000
5000
[cycles], No degradation after
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistance <= 0.30 ohm
<= 0.30 ohm
Shielding Effectiveness 65 dB

@Frequency 1.00e+7 - 3.00e+9 Hz
65 dB

@Frequency 1.00e+7 - 3.00e+9 Hz
Descriptive Properties Value Comments
Color Mid Grey