Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 50 - 60 dB @Thickness 3.00 mm |
50 - 60 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex ZX93134 PPE+PS (Europe-Africa-Middle East) LNP* Faradex* ZX93134 is a compound based on PPE+PS Blend resin containing Stainless Steel Fiber and Glass Fiber. Added features include: Electrically Conductive, EMI/RFI Shielding.This data was su.. |
|||
Shielding Effectiveness | 30 - 60 dB | 30 - 60 dB | 1,000 MHz; PolyOne Internal |
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Shielding Effectiveness | 30 - 60 dB | 30 - 60 dB | 1,000 MHz; PolyOne Internal |
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Shielding Effectiveness | 30 - 60 dB | 30 - 60 dB | 1,000 MHz; PolyOne Internal |
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced
(discontinued **) Data provided by PolyOne. |