Polymer Property : Shielding Effectiveness = 60 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 50 - 60 dB

@Thickness 3.00 mm
50 - 60 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex ZX93134 PPE+PS (Europe-Africa-Middle East)
LNP* Faradex* ZX93134 is a compound based on PPE+PS Blend resin containing Stainless Steel Fiber and Glass Fiber. Added features include: Electrically Conductive, EMI/RFI Shielding.This data was su..
Shielding Effectiveness 30 - 60 dB
30 - 60 dB
1,000 MHz; PolyOne Internal
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Shielding Effectiveness 30 - 60 dB
30 - 60 dB
1,000 MHz; PolyOne Internal
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.
Shielding Effectiveness 30 - 60 dB
30 - 60 dB
1,000 MHz; PolyOne Internal
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced  (discontinued **)
Data provided by PolyOne.