Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 26.0 - 32.0 dB
26.0 - 32.0 dB
Average value: 29.3 dB Grade Count:3
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..