Polymer Property : Shielding Effectiveness = 53 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 53 dB

@Frequency 5.00e+9 Hz
53 dB

@Frequency 5.00e+9 Hz
1/8 thickness
PolyOne Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Shielding Effectiveness 53 dB

@Frequency 100000 Hz
53 dB

@Frequency 100000 Hz
H-Field
P & P Technology VF Series Triple Mesh Dust Filter – Type VH-08
The VH-08 dust filter assemblies are constructed from three layers of corrugated aluminum mesh held in a ‘C’ section aluminum extruded frame. Please see standard profiles available in our catalogu..
Shielding Effectiveness 53 dB

@Frequency 4.00e+7 Hz
53 dB

@Frequency 4.00e+7 Hz
360° Ground Termination
Parker Chomerics CHO-JAC® CJ-021 Flat Cable EMI Shield
Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight ..
Shielding Effectiveness 53 dB

@Frequency 1.00e+8 Hz
53 dB

@Frequency 1.00e+8 Hz
360° Ground Termination
Parker Chomerics CHO-JAC® CJ-021 Flat Cable EMI Shield
Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight ..