Polymer Property : Shielding Effectiveness = 26 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 26 dB

@Frequency 5.00e+9 Hz
26 dB

@Frequency 5.00e+9 Hz
1/8 thickness
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..