PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer PolyOne Corporation
Trade Name Stat-Tech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low to high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.017 - 0.018 cm/cm
0.017 - 0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 86.1 MPa
12500 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 7.18 GPa
1040 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.787 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
228 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Internal Method; UL 94
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Static Decay 0.0020 sec
0.0020 sec
(Mil-B-81705C), 12% RH, 5000kV to 50kV
Shielding Effectiveness 16 dB

@Frequency 1.00e+9 Hz
16 dB

@Frequency 1.00e+9 Hz
1/8 thickness
26 dB

@Frequency 5.00e+9 Hz
26 dB

@Frequency 5.00e+9 Hz
1/8 thickness
36 dB

@Frequency 1.00e+10 Hz
36 dB

@Frequency 1.00e+10 Hz
1/8 thickness
Descriptive Properties Value Comments
Features Electromagnetic Shielding (EMI)
Filler / Reinforcement Nickel-Coated Carbon Fiber
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Aerospace Applications
Automotive Electronics
Computer Components
Connectors
Electrical Housing
Electrical/Electronic Applications
Users viewing this material also viewed the following: