Polymer Property : Shielding Effectiveness = -23.0 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness -23.0 dB

@Thickness 1.57 mm,
Frequency 8.00e+9 Hz
-23.0 dB

@Thickness 0.0620 in,
Frequency 8.00e+9 Hz
Microwave Absorption
Parker Chomerics CHO-MUTE 9000 Microwave Absorber
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon..
Shielding Effectiveness -23.0 dB

@Thickness 1.57 mm,
Frequency 8.00e+9 Hz
-23.0 dB

@Thickness 0.0620 in,
Frequency 8.00e+9 Hz
Microwave Absorption
Parker Chomerics CHO-MUTE 9005 Microwave Absorber
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon..