Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 30 - 80 sec | 30 - 80 sec | ASTM D495 |
Covestro Makrolon® 8325 Polycarbonate High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |